Small stable cracks and holes can often be repaired locally, but hollow, crumbling or damp plaster needs the cause investigating and may require larger areas to be removed. A filler repair cannot make a moving or failed background sound.

Plaster damage ranges from a fine settlement crack to a wall that sounds hollow and moves when pressed. These are not variations of the same repair. Filling the visible line without checking the background often leads to the crack returning or a larger section failing later.

The sensible starting point is to identify what has failed, whether it is still moving and whether moisture is involved. From there you can decide between a local patch, scrim and filler, a skim over a sound wall, or removing defective plaster back to a firm base.

Check safety before disturbing old surfaces

Old plaster and associated textured coatings can contain asbestos, depending on their age and composition. Do not sand, scrape, drill or break out suspect material until it has been assessed and, where appropriate, tested by a competent person. The same caution applies to old Artex on a wall or ceiling above the repair.

Pre-1980s paint may contain lead. Avoid dry-sanding or creating dust from unknown old paint layers. Use suitable testing and controlled preparation methods. Repairs to ceilings, stairwells and high walls should not be tackled with improvised access; use a competent professional with the right equipment.

Hairline cracks or cracks that keep returning

A fine, stable crack in an otherwise firm wall may only need opening out slightly, cleaning and filling with a suitable repair material. Cracks along plasterboard joints can require joint tape and a wider feathered repair so the finished surface does not show a raised line.

A wide crack, one that steps through masonry, or one that repeatedly returns can indicate ongoing movement. Differences between old and new materials can also cause cracking at junctions. Do not assume a decorative filler solves structural movement. Where the pattern or extent is concerning, arrange an appropriate building assessment before repairing the surface.

Panelling joints have their own causes and repairs, explained separately in our guide to cracks at panelling joints.

Read our cracks at panelling joints.

Repairing small and large holes

Small fixing holes need loose material removed and a filler suited to their depth. Deep voids generally need building up in stages or backing with a suitable repair patch rather than one heavy fill that shrinks and cracks. The edges of the surrounding plaster must be firm before the patch is applied.

Larger holes through plasterboard or broken lath-and-plaster need a proper supported repair. Simply pressing filler into an unsupported cavity leaves a weak surface. Once repaired and dry, the area is sanded and feathered carefully so it sits flush without a visible island under the paint.

What blown or crumbling plaster means

Blown plaster has separated from the wall behind it. It often sounds hollow when tapped and may bulge or crumble at the edges. A skim over the top does not restore that bond. The failed area needs removing back to sound material and rebuilding with a compatible backing system before finishing.

On older solid-wall buildings, material choice matters. A hard, impermeable patch is not always suitable next to traditional lime plaster. The repair should suit the construction and allow the wall to manage moisture appropriately rather than trapping it behind a new surface.

Read our checking whether plaster is sound before panelling.

Deal with damp before repairing the finish

Brown staining, salt deposits, mould and soft plaster are signs to investigate moisture rather than simply fill and paint. Possible sources include leaks, penetrating rain, plumbing faults, condensation and bridging of a damp-proof course. Each requires a different remedy.

Let the source be corrected and the wall dry before deciding how much plaster to replace. Stain-blocking paint may hide a mark temporarily but does not dry out a failed wall. Panelling or fitted furniture fixed over a damp background can conceal the problem while timber and board materials absorb moisture.

When a skim or full replaster makes more sense

Lots of shallow surface defects across an otherwise sound wall can make a full skim more practical than dozens of separate patches. Skimming is a finishing process, however, and still needs a stable, properly prepared background. It is not a cure for blown backing plaster or active damp.

If you are preparing for panelling, only the visible areas may need a decorative finish, but the whole fixing surface still needs to be sound and dry. Compare the scope carefully when obtaining prices. Our plastering cost guide explains why preparation and background condition affect the quote.

Do not sand or scrape old Artex to prepare a repair without testing it first; safe professional advice comes before any disturbance.

Read our plastering cost guide.

Want a professional to handle it?

Send us a message

Tell us what you have in mind and we will come back to you.

If it is urgent, call Bradley on 07833 227576.

 

Common questions

Can I fill a crack in plaster and paint straight away?
Only after the repair material has dried for the time stated by its manufacturer and has been prepared for paint. If the crack is moving, widening or linked to damp, filling alone is unlikely to last.
How do I know if plaster is blown?
A hollow sound, movement under gentle pressure, bulging and crumbling edges can all indicate loss of bond. A competent plasterer should confirm the extent before a repair is specified.
Should a damaged wall be skimmed or replastered?
Skimming suits a sound background that needs a new smooth finish. Loose, hollow, wet or crumbling backing plaster normally needs removing and rebuilding before the finish coat.
Can damaged plaster be covered with panelling?
Panelling can hide cosmetic unevenness, but the wall must still provide sound fixings and be free from unresolved damp or movement. Covering a defect is not the same as repairing its cause.

Read next

Related services

Covering Hampshire

Tell us what you have in mind

Send a few details, or call Bradley on 07833 227576 or 02380 201687. We cover Hampshire and the area around it.

MobileLandlineEmailGet a quote